Stainless steel for seawater means the super duplex and super austenitic families, because 316 rusts in seawater, especially around hard fouling and crevices. Super austenitic grades are austenitic grades with about 6 percent molybdenum, and none is in the tables here. Seawater carries chloride ions, which attack the passive layer on stainless steel. PREN, the pitting resistance equivalent number, ranks grades by chemistry, but it is only an indication of resistance.
PREN by grade at a glance
PREN, calculated from minimum composition, scale 0 to 40
- 316 in seawater
- Rusts, especially around hard fouling and crevices
- Super duplex S32750 and S32760
- Avoid prolonged exposure above 250 °C
S32750 and S32760 are super duplex grades. 904L is used in seawater handling, desalination and marine heat exchangers.
What Is PREN and How Is It Calculated?
PREN is calculated as %Cr + 3.3 x %Mo + 16 x %N, where Cr is chromium, Mo is molybdenum and N is nitrogen, each in percent by weight.
A higher number means more resistance to pitting. Pitting is the formation of small, deep holes in the metal surface. The calculated PREN only gives an indication of the resistance of stainless steels, and it gives no information on behaviour in a real environment. Use it to compare grades, never to predict life.
| Grade | Calculated from minimum composition | Producer figure |
|---|---|---|
| 304L | 17.5 | none stated |
| 316L | 22.6 | none stated |
| 317L | 27.9 | greater than 28 |
| 904L | 32.2 | 34 minimum |
| Duplex 2205 | 34.1 | about 35 |
| Super duplex S32760 | 37.1 | 40 minimum |
| Super duplex S32750 | 37.7 | above 40 |
The calculated column uses the lowest chromium, molybdenum and nitrogen the grade limits allow. The producer column is the figure each producer states for its product, so the two columns can differ. Our stainless steel PREN calculator runs the same formula on any composition.
Why Does Seawater Corrode Stainless Steel?
Seawater corrodes stainless steel because chloride ions break down the passive layer and start pitting and crevice corrosion.
Crevice corrosion is attack inside a narrow gap, for example under a gasket, a deposit or hard marine fouling. Stainless steels are particularly susceptible in media with chloride ions. Molybdenum and nitrogen raise pitting resistance, which is why they sit in the PREN formula. Chloride also causes stress corrosion cracking, which is cracking under tensile stress. In 304 and 316 it needs tensile stress and a temperature above about 50 °C. Cracking can occur lower, about 30 °C, in indoor swimming-pool air. Super duplex and super austenitic grades handle high-chloride environments up to nearly boiling point.
Which Stainless Grades Suit Seawater?
Super duplex S32750 and S32760 and super austenitic grades suit seawater. 316 rusts in seawater, especially around hard fouling and crevices.
| Grade | Position for seawater and chloride |
|---|---|
| 304 and 316 | Not suited: 316 rusts in seawater, especially around hard fouling and crevices |
| Lean duplex (less alloyed than 2205) | Pitting and crevice resistance similar to, or just below, 316L |
| Duplex 2205 | Pitting and crevice resistance similar to 904L; used in desalination |
| 904L | Used in seawater handling, desalination and marine heat exchangers |
| Super duplex S32750 | Used on offshore platforms in heat exchangers, process and service water, firefighting, injection and ballast water; also desalination |
| Super duplex S32760 | Used in seawater and offshore systems and in desalination |
Super duplex is essentially equivalent in pitting and crevice resistance to the 6 percent molybdenum super austenitic grades. In cold seawater, 2205 may be an alternative where severe crevice designs are avoided. Cold seawater has no stated temperature, so the duty decides.
Super duplex S32750 sheets and plates and super duplex S32760 plates are the two super duplex products. For the step between duplex and super duplex, see duplex and super duplex compared. Details of 904L stainless steel sheets and plates and duplex 2205 sheets and plates are on their product pages.
Where Does 316L Fit Near the Sea?
316 and 316L suit urban air, including light marine-influenced or polluted air, and are not presented here as seawater grades.
Chlorides are the primary driver of atmospheric corrosion, and coastal areas are particularly aggressive. 316L sheets and plates carry about 2 to 3 percent molybdenum, which helps against chloride exposure in air. Sources conflict on 316L for immersed or splash duty, so send the duty before choosing it.
What Do CPT and CCT Mean?
CPT is the critical pitting temperature and CCT is the critical crevice temperature: the lowest test temperature at which pitting or crevice attack starts in a stated solution.
ASTM G48 covers ferric chloride pitting and crevice tests. ASTM G48 methods E and F give the critical pitting and critical crevice temperature for stainless steels. The figures in the table are laboratory results with their conditions. Service limits are different, and no seawater temperature rule was found for any grade.
| Grade | Test result and condition |
|---|---|
| 904L | Mean CPT around 75 °C at 400 mV SCE (millivolts against a saturated calomel electrode), pH 6, in a solution with the chloride content of seawater |
| 904L | No crevice attack at 50, 60 and 70 °C in aerated stagnant NaCl solution, 1.8 percent Cl-, pH 6, 58 days |
| 316L | Attacked at 50 °C (38 percent) and 60 °C (21 percent) in the same crevice test |
| Super duplex S32750 | CCT of 64 °C in natural seawater at 150 mV vs SCE, temperature raised in 4 °C steps every 24 hours |
The 904L and 316L results come from tube material tested by one producer. The S32750 result is for one tube. A different solution, surface or crevice design gives a different figure.
How Do Seawater Zones Change the Choice?
The zone decides: coastal air, splash, submerged and heat exchanger coolant duties each stress the steel differently.
Cathodic protection is a method of protecting metal by making it the negative electrode in an electrical circuit.
| Zone | What matters |
|---|---|
| Coastal air | Chlorides are the main driver; 316 and 316L suit light marine-influenced air |
| Splash zone | Cathodic protection is not reliable, because the steel is not in continuous contact with seawater |
| Submerged | Chloride content, temperature, dissolved oxygen, pollutants and microbiological activity |
| Heat exchanger coolant | Super duplex tube is used with seawater or chlorinated seawater as coolant |
Design matters as much as grade: gaskets, deposits and fouling create crevices on any steel.
What Temperature Limits Apply to These Grades?
Duplex 2205 is used from -40 °C to 300 °C, 904L from -60 °C to 400 °C, and super duplex should avoid prolonged exposure above 250 °C.
Above 250 °C, super duplex changes microstructure and loses impact strength. The limits come from metallurgy, not from seawater.
How Does Cost Compare Between Seawater Grades?
Cost rises with the nickel and molybdenum in the grade, and what decides stainless steel price sets out the factors.
For current rates see the duplex 2205 plate price list.
We supply super duplex S32750 and S32760 plate and 904L sheets and plates from Mumbai, and a mill test certificate comes with every supply. We can check the duty with you before a grade is quoted. Send the water, the temperature, the crevice details and the quantity.
Frequently Asked Questions
What Is the Best Stainless Steel for Seawater?
Super duplex S32750 or S32760 and super austenitic grades suit seawater; 316 rusts in it. The right choice depends on zone, temperature and crevice design. Send the duty and we will check it with you.
Is 316L Good for Seawater?
No, not as a general rule. 316 rusts in seawater, especially around hard fouling and crevices. 316L suits urban and light marine-influenced air, and immersed duty needs a check of the actual conditions.
What PREN Is Needed for Seawater?
No standard figure was found. PREN only gives an indication of resistance, and zone, temperature and design change the answer. The 904L, 2205 and super duplex values are in the PREN table above.
Is 904L Suitable for Seawater?
Yes, for seawater handling, desalination and marine heat exchangers. In a crevice test at 1.8 percent Cl- and pH 6, 904L showed no initiated attack at 50, 60 and 70 °C, while 316L was attacked at 50 and 60 °C.
Is Duplex 2205 Suitable for Seawater?
Yes, in some cases. Duplex 2205 is used in desalination, and in cold seawater it may be an alternative where severe crevice designs are avoided. The duty decides whether it is enough.
How Much Chloride Can 316L or 304 Take?
No official safe figure in parts per million was found. Producers give temperature limits and test results, not a safe chloride table. Stress corrosion cracking of 304 and 316 needs tensile stress and a temperature above about 50 °C.
Does PREN Predict How Long Stainless Steel Lasts?
No, PREN does not predict life. PREN compares chemistry only and gives no information on behaviour in real environments. Test figures such as CPT and CCT carry the solution and temperature that produced them.