Skip to content
Ostrava Metals

Grade comparison

201 vs 202 vs 304 Stainless Steel

Choose 304 stainless steel for kitchens, damp areas and interior and light urban air, and 201 or 202 only for dry indoor work where price per kg decides the order. Nickel separates the three grades: 304 holds 8.0 to 10.5 percent, 202 holds 4.0 to 6.0 percent and 201 holds 3.50 to 5.50 percent. The 200-series grades carry 5.50 to 10.0 percent manganese, against 2.00 percent maximum in 304. Lower nickel cuts the price per kg, and it also lowers corrosion resistance. Strength is the one property where 201 and 202 match or beat 304.

201, 202 and 304 at a glance

Nickel, % by weight

2013.50 to 5.50
2024.0 to 6.0
3048.0 to 10.5

Manganese, % by weight

2015.50 to 7.50
2027.5 to 10.0
3042.00 max

Choose 201 or 202 for

  • Dry indoor parts where price per kg sets the budget

Choose 304 for

  • Kitchen equipment and food-handling equipment
  • Damp areas and cleaning chemicals
  • Interior and light urban air
Nickel of 6.0 % or less with manganese of 5.50 % or more points to 201 or 202. Scale for all bars: 0 to 12 %.

Difference Between 201, 202 and 304 Stainless Steel

The difference between 201 and 304 is nickel and manganese: 304 has 8.0 to 10.5 percent nickel and 2.00 percent manganese maximum, while 201 and 202 have less nickel and 5.50 to 10.0 percent manganese.

Limits for 201 (UNS S20100) and 304 (UNS S30400) follow ASTM A240. The 202 (UNS S20200) limits are mill specification values.

Element201202304
C (Carbon)0.15 max0.150 max0.07 max
Mn (Manganese)5.50 to 7.507.5 to 10.02.00 max
Cr (Chromium)16.0 to 18.017.00 to 19.0017.5 to 19.5
Ni (Nickel)3.50 to 5.504.0 to 6.08.0 to 10.5
N (Nitrogen)0.25 max0.25 max0.10 max

All values in % by weight.

Nickel is the costly element. 201 is a cost-effective austenitic grade with lean nickel content, and 202 is more affordable than 304 because of its reduced nickel. Austenitic grades are the nickel-bearing family that shows no magnet pull when annealed. The full chemistry of each grade is on the 201, 202 and 304 sheet and plate pages: 201 stainless steel sheets and plates, 202 sheets and plates and 304 sheets and plates.

Corrosion Resistance and PREN

304 stainless steel resists corrosion better than 201 and 202. Low-nickel 200-series grades have less corrosion resistance than grade 304, and failures have occurred in some applications.

PREN is the pitting resistance equivalent number, worked out as %Cr + 3.3 x %Mo + 16 x %N. A higher number means better resistance to pitting, which is local corrosion in chloride (salt) conditions.

GradeChromium (%)Molybdenum (%)PREN (calculated from minimum composition)
20116.0none16.0
20217.00none17.0
30417.5none17.5

PREN is a rough comparison only. The figure gives no information on behaviour in real environments, and it is worked out here with no nitrogen counted, because the minimum nitrogen is not specified.

201 has corrosion resistance comparable to 301-grade steel, which is a different grade from 304. 202 suits budget, indoor, low-corrosion projects, while 304 offers superior corrosion resistance to 202 in industrial service. Chlorides are the primary driver of atmospheric corrosion, and coastal and urban air is particularly aggressive. Guidance for 304 covers interior and light urban air. Coastal and marine-influenced air needs 316, as set out in 304 vs 316 stainless steel.

Strength of 201, 202 and 304

201 and 202 have higher minimum tensile and yield strength than 304, and all three have the same minimum elongation of 40 percent.

Property201 (type 201-2)202304
Tensile strength655 MPa min620 MPa min515 MPa min
Yield strength310 MPa min260 MPa min205 MPa min
Elongation40 % min40 % min40 % min
Hardness100 HRB max100 HRB max92 HRB max

Values are for annealed sheet. The 201 values apply to type 201-2 only. HRB is the Rockwell B hardness scale.

Higher strength does not make 201 or 202 the safer choice. Strength decides thickness and load; corrosion resistance decides service life in wet or salty conditions.

Does a Magnet Identify 201, 202 or 304?

No, a magnet alone does not identify 201, 202 or 304. Annealed austenitic stainless steel shows no pull, but welded 304 often attracts a magnet lightly even though the base metal is non-magnetic.

Some austenitic grades also become mildly magnetic after cold working, depending on composition. A weak pull therefore says nothing about nickel content. The reliable check is the mill test certificate, which prints nickel and manganese for the heat. A strongly magnetic sheet is a different family, such as the ferritic grade compared in 430 vs 304 stainless steel.

Where Are 201, 202 and 304 Used?

201 serves small appliances, catering equipment and cooking utensils. 202 serves cookware, sinks, wire mesh and railway rolling stock. 304 covers the widest set:

  • utensils, cookware and sinks (kitchen)
  • food-handling equipment and food processing machinery in dairies, breweries and conveyors (food processing)
  • handrails, revolving doors and architectural fittings (construction)
  • domestic appliances (home appliances)
  • transport, chemical, petrochemical and fertiliser plant equipment (industrial)

The 200-series uses are utensils, appliance parts and catering equipment. The 304 list adds chemical and petrochemical duty, and 304 suits moisture and chemical service.

Which Costs More, 201, 202 or 304?

304 costs more than 201 and 202 because it holds 8.0 to 10.5 percent nickel, against 3.50 to 5.50 percent in 201 and 4.0 to 6.0 percent in 202. Nickel is the costly element, so each step down in nickel lowers the price per kg.

202 is more affordable than 304 because of its reduced nickel, and 201 is a cost-effective grade with lean nickel content. Nickel price, thickness, finish, quantity and cut-to-size work move the rate for each grade. The stainless steel sheet price per kg page shows the current indicative range, and the 201 sheet price list, 202 sheet price list and 304 sheet price list give it grade by grade.

How to Confirm the Grade on the Certificate

The mill test certificate confirms the grade through nickel and manganese: 304 shows nickel of 8.0 to 10.5 percent and manganese of 2.00 percent maximum.

Nickel of 6.0 percent or less with manganese of 5.50 percent or more points to 201 or 202. Manganese of 5.50 to 7.50 percent matches 201, with nickel of 3.50 to 5.50 percent. Manganese of 7.5 to 10.0 percent matches 202, with nickel of 4.0 to 6.0 percent. We supply a mill test certificate with every order, so the lot can be checked against these limits before acceptance.

How to Choose Between 201, 202 and 304

The choice between SS 201, SS 202 and SS 304 follows the service: choose 304 when the part meets water, food, cleaning chemicals or interior and light urban air, and choose 201 or 202 only for dry indoor parts where the lower price per kg matters more than corrosion margin.

ServiceGrade to order
Dry indoor parts, budget set by price per kg202 or 201
Kitchen equipment and food-handling equipment304
Damp areas, cleaning chemicals304
Interior and light urban air304
Coastal or marine-influenced air316

The stainless steel grade selector covers other grades, and buyers can send the service conditions and thickness to us for a grade recommendation.

Frequently Asked Questions

Is 202 Better Than 201?

No, 202 is not clearly better than 201. 202 has more chromium (17.00 to 19.00 percent against 16.0 to 18.0 percent) and a PREN of 17.0 against 16.0, while 201 has the higher strength minimums.

Which Is Better, 201 or 304?

304 is better where corrosion resistance matters, and 201 is better where price per kg decides. 304 has 8.0 to 10.5 percent nickel against 3.50 to 5.50 percent in 201.

Will 201 Rust?

Yes, 201 can corrode in wet or salty service. Grade 201 has a PREN of 16.0, and low-nickel 200-series grades have less corrosion resistance than 304. Chlorides are the primary driver of atmospheric corrosion, so coastal air needs 316 and light urban air suits 304.

Are 201 and 202 Suitable for Outdoor Use?

No, 202 suits budget, indoor, low-corrosion projects, and low-nickel 200-series grades have less corrosion resistance than 304, with failures in some applications. Guidance covers 304 for interior and light urban air and 316 for coastal air.

Can 202 Be Used for Kitchen Items?

Yes, 202 is used for cookware and sinks, and 201 for cooking utensils. 304 is also used for kitchen equipment and food-handling equipment, and it has the higher corrosion resistance of the three.

Is 201 Cheaper Than 304?

Yes, 201 costs less than 304 because it holds 3.50 to 5.50 percent nickel against 8.0 to 10.5 percent. The gap follows the nickel price, which moves with the market, and the price pages show the current range.

Contact Ostrava Metals

Get a Quote