Choose 316 stainless steel where the part meets chlorides, acids or coastal air, and 304 stainless steel for kitchens, food equipment and general fabrication. The deciding element is molybdenum: 316 contains 2.00 to 3.00 percent, and 304 specifies none. Nickel is also higher in 316, at 10.00 to 14.00 percent against 8.0 to 10.5 percent. The pitting resistance number (PREN) rises from 17.5 for 304 to 22.6 for 316. Minimum tensile strength is 515 MPa for both grades, so the extra cost buys corrosion resistance and not strength.
304 and 316 at a glance
Chromium, % by weight
Nickel, % by weight
Molybdenum, % by weight
Choose 304 for
- Kitchen equipment, utensils, sinks
- Interior and light urban architecture
Choose 316 for
- Urban air with light marine influence or pollution
- Boat fittings, deck hardware, coastal components
- Chemical and petrochemical equipment with chlorides or acids
- Surgical instruments and medical devices
Difference Between 304 and 316 Stainless Steel
The difference between 304 and 316 is molybdenum: 316 has 2.00 to 3.00 percent, 304 has none specified, and 316 also has more nickel and less chromium.
Limits follow ASTM A240 for 304 (UNS S30400, EN 1.4301) and 316 (UNS S31600, EN 1.4401).
| Element | 304 | 316 |
|---|---|---|
| C (Carbon) | 0.07 max | 0.08 max |
| Mn (Manganese) | 2.00 max | 2.00 max |
| Si (Silicon) | 0.75 max | 0.75 max |
| P (Phosphorus) | 0.045 max | 0.045 max |
| S (Sulphur) | 0.030 max | 0.030 max |
| Cr (Chromium) | 17.5 to 19.5 | 16.00 to 18.00 |
| Ni (Nickel) | 8.0 to 10.5 | 10.00 to 14.00 |
| Mo (Molybdenum) | not specified | 2.00 to 3.00 |
| N (Nitrogen) | 0.10 max | 0.10 max |
All values in % by weight.
Molybdenum gives 316 a superior edge against chloride exposure. The higher nickel content adds to the cost. The sheet and plate details are on the 304 stainless steel sheets and plates and 316 stainless steel sheets and plates pages.
Chloride and Pitting Resistance
316 stainless steel resists chlorides better than 304. Chlorides occur in seawater and process solutions, and stainless steel is particularly susceptible to pitting and crevice corrosion there.
Pitting is corrosion in small pits, and crevice corrosion attacks narrow gaps. Molybdenum and nitrogen both raise pitting resistance. PREN adds them up as %Cr + 3.3 x %Mo + 16 x %N.
| Grade | Chromium (%) | Molybdenum (%) | PREN (calculated from minimum composition) |
|---|---|---|---|
| 304 | 17.5 | none | 17.5 |
| 316 | 16.00 | 2.00 | 22.6 |
For 316, the sum is 16.00 + 3.3 x 2.00 = 22.6. Nitrogen is counted as zero because no minimum is specified. PREN is a rough comparison only, and it gives no information on behaviour in real environments.
Which Environment Suits 304 and 316?
304 suits interior and light urban air, and 316 suits urban air with light marine influence or pollution. Chlorides are the primary driver of atmospheric corrosion, and coastal and urban areas are particularly aggressive.
Neither grade is immune. 304 and 316 can both suffer stress corrosion cracking in chloride environments above about 50 °C under tensile stress. Hot chloride service under tensile load needs a grade review, and we can check it against the duty.
Strength of 304 and 316 Compared
304 and 316 have the same minimum tensile strength of 515 MPa and the same minimum yield strength of 205 MPa, so 316 is not stronger than 304 on the specification.
| Property | 304 | 316 |
|---|---|---|
| Tensile strength | 515 MPa min | 515 MPa min |
| Yield strength | 205 MPa min | 205 MPa min |
| Elongation | 40 % min | 40 % min |
| Hardness | 92 HRB max | 95 HRB max |
| Density | 7.90 g/cm³ | 8.03 g/cm³ |
Values are for annealed sheet and plate. HRB is the Rockwell B hardness scale.
Welding 304 and 316
304 stainless steel has excellent weldability and good ductility, while 316 needs post-weld annealing in heavy sections to restore corrosion resistance.
316 carries up to 0.08 percent carbon. The higher carbon is the reason for the annealing step. Low-carbon versions limit carbon to 0.030 percent maximum and avoid that step. The difference is set out in the guide to low-carbon 304L and 316L grades.
Where Are 304 and 316 Used?
304 serves everyday and general-purpose work, and 316 serves chloride, acid and coastal work. 304 is the most specified stainless grade: with 304L it makes up more than half of world stainless production.
304 applications:
- utensils, cookware, sinks and appliances (kitchen)
- food processing machinery in dairies, breweries and conveyors (food processing)
- handrails, revolving doors and architectural fittings (construction)
- transport, chemical, petrochemical and fertiliser equipment (industrial)
316 applications:
- chemical processing equipment, petrochemical and oil and gas equipment (industrial)
- surgical instruments and medical devices (medical)
- boat fittings, deck hardware and coastal architectural components (marine and coastal)
In kitchens, 304 suits everyday home cooking, while 316 suits acid contact and industrial food settings.
Which Costs More, 304 or 316?
316 costs more than 304 because it contains 2.00 to 3.00 percent molybdenum and more nickel, 10.00 to 14.00 percent against 8.0 to 10.5 percent. The molybdenum is the main reason for the higher cost, and it buys the higher chloride resistance.
Nickel and molybdenum prices, thickness, finish, quantity and cut-to-size work move the rate for each grade. The stainless steel sheet price per kg page shows the current indicative range, and the 304 sheet price list and 316 sheet price list give it grade by grade.
How to Choose Between 304 and 316
Choose 304 for dry, interior and light urban service, and choose 316 for chloride, acid, marine-influenced or polluted service. The choice between SS 304 and SS 316 follows the environment, not the load.
| Service | Grade to order |
|---|---|
| Kitchen equipment, utensils, sinks | 304 |
| Interior and light urban architecture | 304 |
| Urban air with light marine influence or pollution | 316 |
| Boat fittings, deck hardware, coastal components | 316 |
| Chemical and petrochemical equipment with chlorides or acids | 316 |
| Surgical instruments and medical devices | 316 |
| Chloride service above about 50 °C under tensile stress | Grade review, send the duty |
A mill test certificate comes with every supply, and it shows chromium, nickel and molybdenum for the heat. Molybdenum of 2.00 to 3.00 percent confirms 316. Cheaper 200-series options are compared in 201 and 202 against 304, and the stainless steel grade selector covers further grades. Buyers can send the service conditions to us for a grade recommendation.
Frequently Asked Questions
Which Is Better, 304 or 316?
316 is better in chloride, acid and marine-influenced service, and 304 is better on cost. 316 has 2.00 to 3.00 percent molybdenum and a PREN of 22.6 against 17.5, and it costs more because of that molybdenum and its higher nickel.
Is 316 Worth the Extra Cost?
Yes, 316 is worth the extra cost where chlorides, acids or coastal air are present. For dry interior parts, 304 costs less and has the same tensile minimum. The extra cost comes from molybdenum and nickel.
Can 304 Be Used Near the Sea?
No, 304 is not the grade for coastal air. Guidance places 304 in interior and light urban settings and 316 in urban air with light marine influence, and chlorides make coastal areas particularly aggressive.
What Does Molybdenum Do in 316?
Molybdenum raises resistance to pitting in chloride conditions. 316 contains 2.00 to 3.00 percent, and it adds 3.3 PREN points per percent in the PREN formula.
Is 316 Magnetic?
No, annealed 316 is non-magnetic, as annealed austenitic stainless steel shows no magnet pull. Some austenitic grades become mildly magnetic after cold working, and welded 304 often attracts a magnet lightly.
Is 316 Stronger Than 304?
No, the specification values are equal. Both grades have a 515 MPa tensile minimum, a 205 MPa yield minimum and a 40 percent elongation minimum.
What Is 316L and How Does It Differ from 316?
316L is the low-carbon version of 316, with carbon limited to 0.030 percent maximum against 0.08 percent maximum in 316. Its minimum tensile strength is 485 MPa and minimum yield strength 170 MPa, against 515 MPa and 205 MPa for 316.