Skip to content
Ostrava Metals

Grade comparison

430 vs 304 Stainless Steel

Choose 304 stainless steel for food contact, wet areas and interior and light urban air, and 430 stainless steel for interior panels, appliances and trims where nickel cost decides the order. Nickel is the main chemical difference: 430 holds 0.75 percent maximum, while 304 holds 8.0 to 10.5 percent. 430 is ferritic and magnetic, and 304 is austenitic and shows no pull when annealed. 430 costs less than 304 because it lacks nickel.

430 and 304 at a glance

430

Structure
Ferritic
Magnet
Magnetic
Nickel
0.75 % max

Used for

  • Appliance panels, trims, interior decorative parts
  • Kitchen sinks in everyday domestic use

304

Structure
Austenitic
Magnet
No pull when annealed
Nickel
8.0 to 10.5 %

Used for

  • Cookware and food-handling equipment
  • Welded or heavily formed parts
  • Interior and light urban air

Nickel, % by weight, scale 0 to 12 %

4300.75 max
3048.0 to 10.5
A magnet alone does not confirm 304. The mill test certificate gives the nickel for the heat.

Difference Between 430 and 304 Stainless Steel

The difference between 430 and 304 is nickel and structure: 430 is a ferritic grade with 0.75 percent nickel maximum, and 304 is an austenitic grade with 8.0 to 10.5 percent nickel.

Limits follow ASTM A240 for 430 (UNS S43000, EN 1.4016) and 304 (UNS S30400, EN 1.4301).

Element430304
C (Carbon)0.12 max0.07 max
Mn (Manganese)1.00 max2.00 max
Si (Silicon)1.00 max0.75 max
P (Phosphorus)0.040 max0.045 max
S (Sulphur)0.030 max0.030 max
Cr (Chromium)16.00 to 18.0017.5 to 19.5
Ni (Nickel)0.75 max8.0 to 10.5

All values in % by weight.

Ferritic grades lack nickel, which makes them a more cost-effective option. Austenitic grades are highly weldable and easily formed. Sheet and plate details are on the 430 stainless steel sheets and plates and 304 stainless steel sheets and plates pages.

Is 430 Magnetic?

Yes, 430 is magnetic. Grade 430 is popular as a magnetic household stainless steel, used in kitchen appliances and decorative panels.

Annealed 304 shows no magnet pull. Welded 304 often attracts a magnet lightly even though the base metal is non-magnetic, and some austenitic grades become mildly magnetic after cold working. A weak pull on a formed or welded 304 part is therefore normal. The magnet test separates strongly magnetic ferritic steel from austenitic steel, and it cannot confirm 304 on its own. The mill test certificate gives the answer, with nickel of 0.75 percent maximum for 430 and 8.0 to 10.5 percent for 304.

Corrosion Resistance of 430 vs 304

304 resists corrosion better than 430. 430 has moderate corrosion resistance, which is adequate for everyday interior use, and 304 has good resistance to pitting and crevice corrosion.

PREN is the pitting resistance equivalent number, worked out as %Cr + 3.3 x %Mo + 16 x %N. Neither grade contains molybdenum.

GradeChromium (%)PREN (calculated from minimum composition)
43016.0016.0
30417.517.5

PREN is a rough comparison only, and it gives no information on behaviour in real environments. Nitrogen is counted as zero because no minimum is specified.

Atmospheric guidance puts 430 in interior use and 304 in interior and light urban air. Chlorides are the primary driver of atmospheric corrosion, and coastal and urban areas are particularly aggressive. Coastal work moves up to 316, covered in 304 vs 316 stainless steel. On heat, 430 has good oxidation resistance and performs well in oxidising environments and industrial furnaces. Service limits depend on the grade, the code and the atmosphere, so buyers should send the temperature and duty.

Strength and Hardness Compared

304 has the higher minimum tensile strength at 515 MPa against 450 MPa for 430, and the same yield strength minimum of 205 MPa.

Property430304
Tensile strength450 MPa min515 MPa min
Yield strength205 MPa min205 MPa min
Elongation22 % min40 % min
Hardness89 HRB max92 HRB max
Density7.70 g/cm³7.90 g/cm³

HRB is the Rockwell B hardness scale. The elongation gap, 22 percent against 40 percent, shows how much further 304 stretches before it fractures.

Forming and Welding 430 vs 304

304 forms and welds more easily than 430. Ferritic grades are less formable than austenitic grades, and 430 can be welded but it is more challenging than welding austenitic grades.

430 also has good cold formability. The elongation minimum shows the gap: 22 percent for 430 against 40 percent for 304. 304 has excellent weldability and good ductility. Parts that need extensive forming or welding point to 304, and buyers can send the drawing for a grade check.

Where Are 430 and 304 Used?

430 serves kitchen equipment, appliances and decorative trim, and 304 serves food contact, sinks, cookware and processing equipment.

430 applications:

  • dishwashers, refrigerator interiors and stove trims (home appliances)
  • cutlery and platters (kitchenware)
  • dairy and catering equipment (food service)
  • flue ducts (industrial)
  • decorative architectural elements and domestic panels (construction)
  • automotive components and trims (automotive)

304 applications:

  • utensils, cookware, sinks and appliances (kitchen)
  • food processing machinery in dairies, breweries and conveyors (food processing)
  • handrails, revolving doors and architectural fittings (construction)
  • exhaust systems (automotive)

In kitchens, 430 is a popular choice for sinks, and it gives adequate corrosion resistance for everyday use while keeping costs down. 304 is recommended for everyday home cooking, and 316 is used where acids touch the metal.

Which Costs More, 430 or 304?

304 costs more than 430 because it holds 8.0 to 10.5 percent nickel, while 430 lacks nickel and holds 0.75 percent maximum. Ferritic grades such as 430 are the more cost-effective option for that reason.

Nickel price, thickness, finish, quantity and cut-to-size work move the rate for each grade. The stainless steel sheet price per kg page shows the current indicative range, and the 430 sheet price list and 304 sheet price list give it grade by grade.

How to Choose Between 430 and 304

The choice between SS 430 and SS 304 follows the service: choose 430 for dry interior parts, trims and appliance panels, and choose 304 for food contact, wet areas, welded fabrication and heavily formed parts.

ServiceGrade to order
Appliance panels, trims, interior decorative parts430
Kitchen sinks in everyday domestic use430 or 304
Cookware and food-handling equipment304
Wet areas and food contact304
Welded or heavily formed parts304
Interior and light urban air304
Cheaper 200-series option for dry partsSee 201 and 202 against 304

We supply a mill test certificate with every order, and it shows nickel and chromium for the heat. The stainless steel grade selector covers further grades, and buyers can send the service conditions to us for a grade recommendation.

Frequently Asked Questions

Which Is Better for a Kitchen, 430 or 304?

304 is better for cooking and food contact, and 430 is better where cost matters on sinks and appliance parts. 304 is recommended for everyday home cooking, and 430 gives adequate corrosion resistance for everyday use at a lower cost.

Will 430 Rust?

Yes, 430 can corrode in wet or salty service. Grade 430 has moderate corrosion resistance and a PREN of 16.0, and guidance places it in interior use. Coastal and urban air is particularly aggressive.

Can 430 Be Welded?

Yes, 430 can be welded, but it is more challenging than welding austenitic grades such as 304. 304 is the easier grade to weld.

Does a Magnet Prove a Sheet Is Not 304?

No, a magnet does not prove a sheet is not 304. Welded 304 often attracts a magnet lightly, and cold work can add mild magnetism. Check nickel on the mill test certificate: 8.0 to 10.5 percent for 304.

Why Is 430 Used in Appliances?

430 is used in appliances because it is a magnetic household stainless steel with adequate corrosion resistance for everyday use, at a lower cost since it lacks nickel. Dishwashers, refrigerator interiors and stove trims are the named uses.

Is 430 Cheaper Than 304?

Yes, 430 costs less than 304 because it lacks nickel, 0.75 percent maximum against 8.0 to 10.5 percent in 304. The price pages show the current indicative range for each grade.

Contact Ostrava Metals

Get a Quote