Choose Duplex 2205 where chlorides act on a stressed part or the design needs a higher yield strength, and choose 316L stainless steel where the part needs 40 percent minimum elongation or must stay non-magnetic. Duplex steel 2205 has a minimum yield strength of 450 MPa against 170 MPa for 316L. Its pitting resistance number (PREN) calculates at 34.1 against 22.6.
Duplex 2205 and 316L at a glance
Yield strength, MPa min, scale 0 to 500 MPa
PREN, calculated, scale 0 to 40
- 316L, chloride cracking
- Can crack in chlorides above about 50 °C under tensile stress
- Duplex 2205, service range
- -40 °C to 300 °C
Choose Duplex 2205 for
- Chloride service under tensile stress above about 50 °C, after a duty check
- Design set by yield strength above 170 MPa
- Chemical tanks, desalination, pulp and paper equipment
Choose 316L for
- Parts that must stay non-magnetic when annealed
- Forming that needs 40 percent minimum elongation
- Boat fittings, coastal components, medical devices
The chemistry differs. SS 2205 holds 22.00 to 23.00 percent chromium, 3.0 to 3.50 percent molybdenum and 4.50 to 6.50 percent nickel. SS 316L holds 16.00 to 18.00 percent chromium, 2.00 to 3.00 percent molybdenum and 10.00 to 14.00 percent nickel. Nitrogen is 0.14 to 0.20 percent in 2205 and 0.10 percent maximum in 316L.
Chloride cracking separates the grades in service. 316L can crack in chlorides above about 50 °C under tensile stress, and 2205 resists that cracking better. The service range of 2205 is -40 °C to 300 °C. The steel welds without preheating, and it is strongly attracted by a magnet. Annealed 316L shows no magnet pull. Both grades are supplied as plate and sheet to ASTM A240/A240M.
What Is Duplex 2205 Steel?
Duplex 2205 is a stainless steel with a mixed structure of ferrite and austenite, registered as UNS S32205 (EN 1.4462). UNS is the Unified Numbering System, which gives each alloy a letter and five digits. EN is the European standard number. The S32205 material also meets S31803.
Ferrite and austenite are two crystal structures of steel. Ferrite is magnetic. Annealed austenite shows no magnet pull. Duplex means both structures are present in the same steel.
316L stainless steel (UNS S31603, EN 1.4404) is an austenitic grade. The letter L stands for low carbon, with carbon limited to 0.030 percent maximum. The step from 316 to 316L is set out in the guide to low-carbon 304L and 316L grades, and the step from 304 to 316 in 304 vs 316 stainless steel.
ASTM A240/A240M covers plate, sheet and strip of both grades. Sizes and finishes are on the pages for duplex 2205 sheets and plates and 316L stainless steel sheets and plates.
2205 vs 316L Chemical Composition
SS 2205 holds 22.00 to 23.00 percent chromium against 16.00 to 18.00 for 316L, and less than half the nickel.
Limits follow ASTM A240/A240M for Duplex 2205 (UNS S32205, EN 1.4462) and SS 316L (UNS S31603, EN 1.4404). All values in % by weight.
| Element | Duplex 2205 | 316L |
|---|---|---|
| C (Carbon) | 0.030 max | 0.030 max |
| Mn (Manganese) | 2.00 max | 2.00 max |
| Si (Silicon) | 1.00 max | 0.75 max |
| P (Phosphorus) | 0.030 max | 0.045 max |
| S (Sulphur) | 0.020 max | 0.030 max |
| Cr (Chromium) | 22.00 to 23.00 | 16.00 to 18.00 |
| Ni (Nickel) | 4.50 to 6.50 | 10.00 to 14.00 |
| Mo (Molybdenum) | 3.0 to 3.50 | 2.00 to 3.00 |
| N (Nitrogen) | 0.14 to 0.20 | 0.10 max |
Carbon is the same in both grades, at 0.030 percent maximum. Chromium, molybdenum and nitrogen all enter the PREN formula, so the higher 2205 figures raise its calculated PREN.
Which Is Stronger, 2205 or 316L?
Stainless steel 2205 is stronger: its minimum yield strength is 450 MPa against 170 MPa for 316L, a ratio of 2.6. Yield strength is the stress at which steel starts to deform permanently. Tensile strength is the stress at which it breaks.
| Property | Duplex 2205 | 316L |
|---|---|---|
| Tensile strength | 655 MPa min | 485 MPa min |
| Yield strength (0.2%) | 450 MPa min | 170 MPa min |
| Elongation | 25 % min | 40 % min |
| Hardness | 31 HRC max | 95 HRB max |
| Density | 7.82 g/cm³ | 8.03 g/cm³ |
Values are for annealed plate and sheet. HRC and HRB are the Rockwell C and Rockwell B hardness scales, so the two hardness limits are not compared directly.
The tensile gain is smaller than the yield gain: 655 MPa against 485 MPa is a ratio of 1.35. Producers also state that the yield of 2205 duplex is about twice that of 304 and 316. Elongation runs the other way. The minimum elongation is 40 percent for 316L and 25 percent for 2205, so 316L stretches further before it breaks.
When Does Higher Strength Allow Thinner Plate?
Higher yield strength can allow a lighter construction when strength decides the design, and the design calculation sets how much. Where strength does not set the thickness, the extra strength gives no saving. No standard percentage applies to every design, so the engineer calculates it for the part.
Pitting Resistance and PREN
The PREN of SS 2205 calculates at 34.1 against 22.6 for 316L, so 2205 resists chloride pitting better on this rough comparison. Pitting is corrosion in small pits, and PREN adds up the elements that resist it: PREN = %Cr + 3.3 x %Mo + 16 x %N.
| Grade | Chromium (%) | Molybdenum (%) | Nitrogen (%) | PREN (calculated from minimum composition) | Producer figure |
|---|---|---|---|---|---|
| 316L | 16.00 | 2.00 | none specified | 22.6 | not stated |
| Duplex 2205 | 22.00 | 3.0 | 0.14 | 34.1 | about 35 |
For 2205, the sum is 22.00 + 3.3 x 3.0 + 16 x 0.14 = 22.00 + 9.90 + 2.24 = 34.1. For 316L, the sum is 16.00 + 3.3 x 2.00 = 22.6, with nitrogen counted as zero because no minimum is specified. PREN is a rough comparison only, and it gives no information on behaviour in real environments.
Producers also rate 2205 as having superior corrosion resistance in most media compared with 316L.
Chloride Stress Corrosion Cracking
Duplex steel 2205 resists chloride stress corrosion cracking (SCC) better than 316L, which can crack in chlorides above about 50 °C under tensile stress. SCC is cracking that needs both tensile stress and a corrosive environment, such as hot chloride solution.
Producer test data shows 2205 with a much higher resistance to SCC than 304L and 316L. Hot chloride service under tensile load needs a grade review, and we can check it against the duty.
Temperature Limits of 2205 and 316L
Stainless steel 2205 has a service temperature range of -40 °C to 300 °C. The maximum for SS 316L depends on the code and the atmosphere, so the duty decides it. The grade is checked against the duty that the buyer sends.
Welding 2205 and 316L
SS 316L welds without post-weld heat treatment because its carbon is 0.030 percent maximum; 2205 normally needs none either but requires controlled heat input. Post-weld heat treatment is a heating cycle after welding.
Producer guidance for welding 2205 gives these values:
| Welding item | Duplex 2205 |
|---|---|
| Preheating | not required |
| Post-weld heat treatment | normally not necessary |
| Heat input | 0.5 to 2.5 kJ/mm |
| Interpass temperature | below 150 °C (300 °F) |
| Filler metal | matching over-alloyed filler |
Heat input is the heat put into the weld per millimetre of length. Interpass temperature is the temperature of the weld zone before the next pass starts. An over-alloyed filler is a filler richer in alloying elements than the base metal. An industry body rates the weldability of 2205 at 5 out of 10 and that of 316 at 8 out of 10.
Is Duplex 2205 Magnetic?
Yes, 2205 duplex is magnetic, because its ferrite phase is ferromagnetic and duplex grades are strongly attracted by a magnet. Annealed 316L shows no magnet pull, although cold work can make an austenitic grade mildly magnetic. A magnet alone does not identify the grade.
Can 2205 Replace 316L?
Yes, 2205 replaces 316L where chloride stress or yield strength decides the design, once the engineer has checked four points:
- welding procedure: heat input of 0.5 to 2.5 kJ/mm
- service temperature: within -40 °C to 300 °C
- forming: elongation of 25 percent minimum against 40 percent
- magnetism: the part must tolerate a magnetic steel
A change from 316L to 2205 also changes plate thickness and code approval, so the drawing is reviewed before the order. The wider ladder of duplex and super duplex steels is compared in duplex against super duplex stainless steel.
Plate Standard and Mill Test Certificate
ASTM A240/A240M is the standard for 2205 and 316L plate, sheet and strip, and a mill test certificate comes with every supply. The certificate reports the heat chemical analysis, which is the percentages of the specified elements, and the mechanical test results. ASTM A480/A480M sets the certification and test reports clause for flat-rolled stainless steel.
Check the certificate against the grade limits. On SS 2205, chromium reads 22.00 to 23.00, molybdenum 3.0 to 3.50 and nitrogen 0.14 to 0.20 percent. On 316L stainless steel, molybdenum reads 2.00 to 3.00 percent and carbon 0.030 percent maximum. 2205 is also supplied as coil: see duplex 2205 coils.
Where Are 2205 and 316L Used?
Duplex steel 2205 serves chloride and strength duties in process industries, and SS 316L serves chemical, marine and medical work. Each grade's uses are listed with the industry in brackets.
Stainless steel 2205 applications:
- chemical tanks and process equipment (chemical processing)
- desalination plant equipment (desalination)
- pulp and paper process equipment (pulp and paper)
- heat exchangers and industrial piping (power generation, petrochemical, oil and gas)
- pressure vessels and storage tanks (industrial)
- marine transport equipment (marine)
316L applications:
- chemical and petrochemical equipment (industrial)
- boat fittings and deck hardware (marine and coastal)
- coastal architectural components (construction)
- surgical instruments and medical devices (medical)
Which Costs More, 2205 or 316L?
The indicative market ranges of 2205 and 316L plate and sheet overlap, so neither grade is always cheaper. Nickel is 4.50 to 6.50 percent in 2205 and 10.00 to 14.00 percent in 316L.
Nickel and molybdenum prices, thickness, finish, quantity and cut-to-size work move the rate for each grade. The Duplex 2205 plate price list shows the current indicative range.
How to Choose Between 2205 and 316L
Choose 2205 for chloride service under stress and for strength-led designs, and choose 316L for forming, non-magnetic parts and general chemical or coastal work.
| Service | Grade to order |
|---|---|
| Chloride service under tensile stress above about 50 °C | Duplex 2205, after a duty check |
| Design set by yield strength above 170 MPa | Duplex 2205 |
| Chemical tanks, desalination, pulp and paper equipment | Duplex 2205 |
| Parts that must stay non-magnetic when annealed | 316L |
| Forming that needs 40 percent minimum elongation | 316L |
| Boat fittings, coastal components, medical devices | 316L |
| Service above 300 °C | Grade review, send the duty |
The stainless steel grade selector covers further grades. Buyers can send the service conditions to us, and we reply with a grade recommendation and a quotation.
Frequently Asked Questions
What Is the Main Difference Between Duplex 2205 and 316L?
The main difference is structure and chemistry: 2205 duplex has a ferrite and austenite structure with 22.00 to 23.00 percent chromium, and 316L is austenitic with 10.00 to 14.00 percent nickel. The result is a yield strength of 450 MPa against 170 MPa minimum.
Is 2205 Stronger Than 316L?
Yes, 2205 is stronger. Its minimum yield strength is 450 MPa against 170 MPa, and its minimum tensile strength is 655 MPa against 485 MPa. 316L has the higher elongation, at 40 percent minimum against 25 percent.
Is 2205 More Corrosion Resistant Than 316L?
Yes, in chloride service. The calculated PREN is 34.1 for 2205 and 22.6 for 316L, and producers rate 2205 as superior in most media. PREN is a rough comparison only.
What Is the Difference Between S32205 and S31803?
Both are UNS numbers for 2205 duplex, and the S32205 material also meets S31803. The EN designation of the grade is 1.4462.
Does 2205 Need Post-Weld Heat Treatment?
No, post-weld heat treatment is normally not necessary for 2205, and preheating is not required. The weld needs heat input of 0.5 to 2.5 kJ/mm and an interpass temperature below 150 °C.
What Is the Maximum Temperature for 2205?
The service temperature range of Duplex 2205 is -40 °C to 300 °C. Limits depend on the code and the atmosphere, so send the duty for a check.
Is 316L Magnetic?
No, annealed 316L is non-magnetic and shows no magnet pull. Cold work can make it mildly magnetic, and 2205 is magnetic because of its ferrite.