J4, JT and J204Cu are Jindal's chromium-manganese 200-series stainless steel grades. Jindal lists J4 for deep drawn kitchen equipment, cookware, bins and hoppers, where deep drawn means pressed from flat sheet into cups and bowls. Jindal uses JT for container structures, salt trailers and electric bus tubes. J204Cu is the copper-bearing grade Jindal places between the 200 and 300 series, for kitchenware, sinks and frames.
J4, JT and J204Cu at a glance
Chromium, % by weight, scale 0 to 20 %
Nickel, % by weight, scale 0 to 4 %
Copper, % by weight, scale 0 to 4 %
Manganese, % by weight, scale 0 to 12 %
- J4 made for
- Deep drawn kitchen equipment, cookware, bins and hoppers
- JT made for
- Container structures, salt trailers and electric bus tubes
- J204Cu made for
- Kitchenware, sinks and frames
Nickel runs from 0.5 to 0.95 percent in JT to 1.5 to 3.5 percent in J204Cu, against 8.0 to 10.5 percent in 304. Minimum tensile strength runs from 620 MPa in J204Cu to 700 MPa in JT, against 515 MPa in 304. J4 and J204Cu turn lightly magnetic after cold working, which means bending, rolling or drawing the metal at room temperature. Jindal's cup test gives J4 a limiting drawing ratio of 1.7 against 2.1 for 304. Jindal states that J204Cu has corrosion resistance similar to 304 in mild corrosive media, and it compares JT only with carbon steel. The J4, JT and J204Cu values come from Jindal's data sheets, and the mill test certificate of the lot is the final record.
What Are J4, JT and J204Cu Grades?
J4, JT and J204Cu are Jindal's own names for three chromium-manganese stainless steel grades of the 200 series.
The 200 series is the group of stainless steels, numbered 201, 202 and so on, that hold more manganese and less nickel than 300-series grades such as 304. Jindal's data sheet lists all three under austenitic chromium-manganese grades. Austenitic steel is non-magnetic when annealed, which means softened by a controlled heat treatment. Each name is a Jindal grade designation with a BIS name, which is a grade name of the Bureau of Indian Standards.
What Is J4 Stainless Steel?
J4 stainless steel is a chromium-manganese austenitic steel with moderate amounts of copper, nickel and nitrogen, in Jindal's description. Jindal gives it the BIS name N1.
Jindal says the balance of alloying elements gives J4 an austenitic structure in the annealed condition. Jindal describes J4 as suitable for replacing the chromium-nickel grades 301 and 304 in many applications, and says the manganese and nitrogen additions make the grade more economical while giving good strength and high formability.
The copper in J4 reduces its work hardening rate. Work hardening is the gain in hardness and strength that metal shows as it is bent, pressed or drawn. Jindal states that J4 can display a wide range of mechanical strength depending on the degree of cold working. Jindal J4 comes as hot rolled plates and coil, and as cold rolled coil and sheets.
A variant, J4-16Cr, is described by Jindal as similar to J4 with higher chromium (16.0 to 17.0 percent) for increased corrosion resistance.
What Is JT Grade Stainless Steel?
JT grade stainless steel is a Jindal chromium-manganese grade with 9.0 to 11.0 percent manganese, 13.5 to 15.0 percent chromium and 0.5 to 0.95 percent nickel. Its BIS name is N7.
JT stainless steel has the lowest chromium and nickel of the three grades and the highest minimum strength. Jindal's 200-series brochure does not include JT, so the JT values here come from Jindal's product data sheet. Jindal's JT pages describe the grade through its uses in containers, trailers and buses.
What Is J204Cu Stainless Steel?
J204Cu stainless steel is a chromium-manganese 200-series grade with moderate amounts of nickel, copper and nitrogen, and Jindal gives it the BIS name N2. The names J204Cu and 204Cu mean the same Jindal grade.
Jindal says J204Cu bridges the cost and property gap between the 200 and 300 series. In Jindal's wording, copper improves corrosion resistance and stress corrosion cracking resistance in certain media, and nitrogen increases strength and pitting resistance. Stress corrosion cracking is cracking under tensile stress in a corrosive medium, and pitting is the formation of small holes by chlorides.
J4, JT and J204Cu Composition
J4, JT and J204Cu differ most in manganese, chromium, nickel and copper, and all three hold far less nickel than 304.
The table gives limits in percent by weight. The J4 and J204Cu limits are grade-datasheet values from Jindal's 200-series brochure, the JT limits are from Jindal's product data sheet, and 304 is shown for reference. A dash means no limit is listed.
| Element | J4 | JT | J204Cu | 304 (reference) |
|---|---|---|---|---|
| C (Carbon) | 0.10 max | 0.13 max | 0.10 max | 0.07 max |
| Mn (Manganese) | 8.50 to 10.00 | 9.0 to 11.0 | 6.50 to 9.00 | 2.00 max |
| Si (Silicon) | 0.75 max | 0.75 max | 0.75 max | 0.75 max |
| P (Phosphorus) | 0.08 max | 0.10 max | 0.06 max | 0.045 max |
| S (Sulphur) | 0.010 max | 0.015 max | 0.010 max | 0.030 max |
| Cr (Chromium) | 15.0 to 16.0 | 13.5 to 15.0 | 16.0 to 17.5 | 17.5 to 19.5 |
| Ni (Nickel) | 1.0 to 2.0 | 0.5 to 0.95 | 1.5 to 3.5 | 8.0 to 10.5 |
| Cu (Copper) | 1.50 to 2.00 | 0.4 to 0.8 | 2.00 to 4.00 | - |
| N (Nitrogen) | 0.20 max | 0.10 to 0.20 | 0.10 to 0.25 | 0.10 max |
JT holds the most manganese and the least chromium, nickel and copper. J204Cu holds the most chromium, nickel and copper and the least manganese. J4 sits between the two on chromium, nickel and copper.
Jindal's web data sheet prints different limits for some J4 and J204Cu elements. Jindal also states that specific chemical and mechanical properties can be supplied by mutual agreement. The mill test certificate of the actual lot is the final record of what was delivered.
Strength of J4, JT and J204Cu
JT has the highest minimum strength of the three grades, with 700 MPa tensile and 350 MPa yield, followed by J4 at 650 and 325 MPa and J204Cu at 620 and 310 MPa.
Tensile strength is the load per unit area a sample carries before it breaks. Yield strength is the stress at which the metal starts to bend permanently. MPa (megapascal) is the unit of both. HRB is the Rockwell B hardness scale, and a lower number means softer metal.
| Property | J4 | JT | J204Cu | 304 (reference) |
|---|---|---|---|---|
| Tensile strength | 650 MPa min | 700 MPa min | 620 MPa min | 515 MPa min |
| Yield strength | 325 MPa min | 350 MPa min | 310 MPa min | 205 MPa min |
| Elongation | 40 % min | 40 % min | 40 % min | 40 % min |
| Hardness | 100 HRB max | 100 HRB max | 100 HRB max | 92 HRB max |
All three Jindal grades have higher minimum tensile and yield strength than 304. Elongation, the stretch before fracture, has the same 40 percent minimum in all four columns. Jindal notes that the strength of J4 varies widely with the degree of cold working.
J4 vs 304 Stainless Steel
J4 holds 1.0 to 2.0 percent nickel against 8.0 to 10.5 percent in 304, and Jindal's cup tests show that J4 draws less deeply than 304.
Manganese is the other large difference: J4 holds 8.50 to 10.00 percent and 304 holds 2.00 percent maximum. J4 also has the higher minimum strength, 650 MPa tensile and 325 MPa yield against 515 MPa and 205 MPa. Jindal describes J4 as suitable for replacing 301 and 304 in many applications. For 304 itself, see the 304 sheets and plates page.
Deep Drawing Test Results
Jindal's cup tests give J4 a limiting drawing ratio of 1.7 against 2.1 for 304, and an Erichsen cupping value of 11.5 mm against 13.1 mm.
Deep drawing is pressing flat sheet into a cup or bowl with a punch. The limiting drawing ratio is the largest ratio of flat blank diameter to cup diameter that can be drawn in one step without tearing. The Erichsen cupping value is the depth in millimetres of a dome pressed into the sheet before it cracks. A higher number means a deeper draw in both tests.
| Test | J4 | 304 |
|---|---|---|
| Limiting drawing ratio | 1.7 | 2.1 |
| Erichsen cupping value | 11.5 mm | 13.1 mm |
On these figures, a cup drawn in one step at a ratio above 1.7 is outside the J4 limit but inside the 304 limit. Jindal still lists J4 for deep drawn kitchen equipment, cookware and serving bowls, so the shape and depth of each part decide whether one draw or two is needed.
Cold Forming of J204Cu and JT
J204Cu can take up to 80 percent cold reduction without intermediate annealing, according to Jindal.
Cold reduction is the thinning of metal by rolling or drawing at room temperature, and intermediate annealing is a softening heat treatment between forming steps. Jindal credits the copper in J204Cu with a lower work hardening rate and states better formability than J201 and 304. In its summary of properties, Jindal also lists the formability and weldability of J204Cu as similar to 304. Both are producer statements, so a trial forming of the actual lot settles the question for a difficult part.
Jindal's data gives no deep-drawing or cold-reduction figures for the JT grade. The uses Jindal names for JT are structural: container frames, trailers and bus tubes.
Is J4 Stainless Steel Magnetic?
Yes, J4 stainless steel becomes lightly magnetic after cold working, and it is non-magnetic in the annealed condition, as Jindal states.
Jindal writes that J4, like 304, turns lightly magnetic after cold working because martensite forms. Martensite is a harder, magnetic crystal structure that forms in some austenitic steels when they are deformed. Annealing at about 1050 degrees C followed by rapid water quenching restores the full austenitic structure, according to Jindal's note on austenitic steels in general.
J204Cu also becomes magnetic with cold reduction, because deformation martensite forms. Jindal says the amount of martensite in J204Cu is much less than in 304, and reports 3.0 percent martensite after 67 percent cold work. Jindal's data does not state the magnetic behaviour of JT, so the lot needs its own test if the part must stay non-magnetic.
A magnet therefore cannot name the grade, and it cannot separate the three grades from 201, 202 or 304, as set out in the 201 vs 202 vs 304 stainless steel comparison. A strongly magnetic sheet is a different, ferritic family, such as the 430 grade in 430 vs 304 stainless steel.
Corrosion Resistance of J4, JT and J204Cu
Jindal states that J204Cu has corrosion resistance similar to 304 in a variety of mild corrosive media, and it gives no such comparison for J4 or JT.
Corrosion in J4
J4 has no corrosion comparison with 301 or 304 in Jindal's grade data. Jindal's statement is that J4 is suitable for replacing 301 and 304 in many applications. For jobs that need more corrosion resistance, Jindal offers J4-16Cr, the variant with 16.0 to 17.0 percent chromium.
Corrosion in JT
JT is compared by Jindal with carbon steel only, and the claim is superior corrosion resistance compared to carbon steel. Jindal's data gives no corrosion comparison of JT with 201, 202 or 304, so none is made here.
Corrosion in J204Cu
204Cu stainless steel has the most corrosion data of the three in Jindal's brochure. Jindal states that J204Cu and 304 are immune from intergranular corrosion if properly heat treated, tested to ASTM A262. Intergranular corrosion is attack along the grain boundaries of the metal.
Jindal also reports a food leaching test on J204Cu. Chromium and nickel leaching was below 0.1 ppm in all eight food simulants and in tomato soup, and the samples showed no surface corrosion spot or rust marks and no measurable weight loss. The test is Jindal's own. ppm means parts per million.
Limits to Check Before Use
Industry guidance says low-nickel 200-series grades have less corrosion resistance than 304, and failures have occurred in some applications. Chlorides are the primary driver of atmospheric corrosion, and coastal and urban air is particularly aggressive.
The Jindal data held for J4, JT and J204Cu gives no chloride, marine or outdoor limit. Send the service conditions before ordering for wet, salty or chemical duty.
Where Are J4, JT and J204Cu Used?
Jindal lists J4 for deep drawn kitchen equipment and bins, JT for container structures and trailers, and J204Cu for kitchenware, sinks and frames.
Uses of J4
Jindal names seven uses for the J4 grade:
- deep drawn kitchen equipment
- cookware and serving bowls
- furniture
- bins
- coal buckets
- wear plate liners and hoppers
- window channel spacers
Uses of JT
Jindal's JT pages name four uses:
- container structures, with 2.0 MT of JT sheets and 0.50 MT of JT tubes per container
- railway salt containers (external stiffeners and underframe)
- salt trailers
- JT tubes for electric buses
MT means metric tonne. Jindal states that JT has excellent impact resistance, nearly 2.5 times that of carbon steel, and that its container example saves approximately 500 kilograms of weight.
Uses of J204Cu
Jindal's brochure groups the uses of J204Cu into four fields. Six examples are:
- deep drawn kitchenware and utensils (catering and food process)
- sinks (consumer durables)
- refrigerator outer body parts (catering and food process)
- handrails and door and window frames (architecture)
- automotive hose clamps (transport)
- truck and bus frames (transport)
J4, JT or J204Cu: Which to Choose?
Choose the grade Jindal lists for the job: J204Cu for kitchenware, sinks and frames, J4 for deep drawn kitchen equipment, bins and hoppers, and JT for containers, trailers and bus tubes.
| Job | Grade | Basis in Jindal's data |
|---|---|---|
| Deep drawn utensils and cookware | J204Cu or J4 | Both listed; J4 limiting drawing ratio is 1.7 |
| Sinks and oven outer parts | J204Cu | Listed under consumer durables |
| Refrigerator outer parts | J204Cu | Listed under catering and food process |
| Handrails, door and window frames | J204Cu | Listed under architecture |
| Bins, hoppers, wear plate liners, furniture | J4 | Listed for J4 |
| Containers, salt trailers, electric bus tubes | JT | Listed for JT |
| Hose clamps, truck and bus frames | J204Cu | Listed under transport |
| Highest minimum strength | JT | 700 MPa tensile, 350 MPa yield |
On cost, Jindal states that the manganese and nitrogen in J4 make it more economical than 301 and 304, and that J204Cu suits jobs that need higher strength and high formability at lower cost. We give no price order among the three, because Jindal's data gives none.
Parts that meet water, cleaning chemicals or interior and light urban air are the jobs our 201 vs 202 vs 304 comparison assigns to 304. The stainless steel grade selector covers the other grades.
How to Check the Mill Certificate
A mill test certificate confirms the grade through the heat's chemical analysis and mechanical test results, which the buyer compares with the grade limits.
Four checks identify the grade:
- Read the copper value first: JT shows 0.4 to 0.8 percent, J4 shows 1.50 to 2.00 percent and J204Cu shows 2.00 to 4.00 percent.
- Compare chromium: J204Cu shows 16.0 to 17.5 percent, J4 shows 15.0 to 16.0 percent and JT shows 13.5 to 15.0 percent.
- Compare nickel and manganese with the composition table above.
- Compare tensile and yield strength with the minimums in the strength table.
A value on an edge, such as 2.00 percent copper, belongs to either J4 or J204Cu, so read the grade name and the other elements with it. Check the limits agreed on the order as well, because Jindal supplies specific properties by mutual agreement.
Frequently Asked Questions
Is J4 Stainless Steel Good for Utensils?
Yes, Jindal lists J4 for deep drawn kitchen equipment and for cookware and serving bowls. J4 draws less deeply than 304, with a limiting drawing ratio of 1.7 against 2.1, so a deep cup may need a shallower draw. The food leaching results in Jindal's brochure are for J204Cu, not J4.
What Is the Difference Between J4 and 202?
J4 has less chromium and nickel than 202 and higher minimum strength. J4 holds 15.0 to 16.0 percent chromium and 1.0 to 2.0 percent nickel, against 17.00 to 19.00 percent and 4.0 to 6.0 percent in Jindal's J202. Minimum tensile and yield strength are 650 and 325 MPa for J4 and 620 and 260 MPa for J202. Jindal gives no J4 against 202 corrosion comparison. See the 202 sheets and plates page for the full 202 data.
Which Is Stronger, JT or 201?
JT is stronger, with minimums of 700 MPa tensile and 350 MPa yield against 655 MPa and 310 MPa for 201 type 201-2 (Jindal J201). JT also holds less nickel (0.5 to 0.95 percent against 3.50 to 5.50 percent) and less chromium (13.5 to 15.0 percent against 16.0 to 18.0 percent). Jindal gives no JT against 201 corrosion comparison. The 201 sheets and plates page lists the 201 data.
Can J204Cu Replace 304?
Yes, Jindal states that J204Cu can replace type 304 in numerous applications where higher strength, high formability and lower cost are required. Jindal rates the corrosion resistance of J204Cu as similar to 304 in a variety of mild corrosive media. J204Cu holds 1.5 to 3.5 percent nickel against 8.0 to 10.5 percent in 304, so a wet or salty service needs checking first.
Does JT Stainless Steel Contain Nickel?
Yes, Jindal's data sheet gives JT 0.5 to 0.95 percent nickel. The same sheet gives 13.5 to 15.0 percent chromium, 9.0 to 11.0 percent manganese and 0.4 to 0.8 percent copper. Read the nickel value on the mill test certificate of the lot.
Which Standard Covers J4, JT and J204Cu?
Jindal names no ASTM standard for J4, JT or J204Cu; it lists them as its own grades with the BIS names N1, N7 and N2. BIS is the Bureau of Indian Standards. Jindal states that JT is designated as JT or N7 under the BIS 6911 specification, so a quotation that says N7 grade means JT.
Ask About Jindal Grades
We are an authorised Jindal Stainless dealer in Mumbai, and a mill test certificate comes with every supply. Send the grade name on your quotation, the thickness and the job to info@ostravametals.com, or use the contact page, and we will check the grade against Jindal's data.